Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.125 GPa @Strain 21.63 %, Temperature -40.0 °C |
18.1 ksi @Strain 21.63 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |