Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 175.40 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.2093 GPa

@Strain 4.30 %,
Temperature 0.000 °C
175.40 ksi

@Strain 4.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..
Copyright © lookpolymers.com All Rights Reserved