Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 10.7 GPa @Strain 0.140 %, Temperature 40.0 °C |
1550 ksi @Strain 0.140 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Secant Modulus | 10.7 GPa @Strain 2.10 %, Temperature 23.0 °C |
1550 ksi @Strain 2.10 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |