Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 152.085 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.04857 - 6.80 GPa

@Temperature -40.0 - 100 °C
152.085 - 986 ksi

@Temperature -40.0 - 212 °F
Average value: 3.63 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Secant Modulus 1.04857 - 6.80 GPa

@Strain 0.250 - 3.50 %
152.085 - 986 ksi

@Strain 0.250 - 3.50 %
Average value: 3.63 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Copyright © lookpolymers.com All Rights Reserved