Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 10.4 GPa @Strain 0.580 %, Temperature 0.000 °C |
1510 ksi @Strain 0.580 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Secant Modulus | 10.4 GPa @Strain 1.58 %, Temperature 0.000 °C |
1510 ksi @Strain 1.58 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Secant Modulus | 10.4 GPa @Strain 0.880 %, Temperature -40.0 °C |
1510 ksi @Strain 0.880 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |