Mechanical Properties Metric English Comments
Secant Modulus 1.70799 - 14.8867 GPa

@Temperature 0.000 - 200 °C
247.727 - 2159.17 ksi

@Temperature 32.0 - 392 °F
Average value: 10.1 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Secant Modulus 1.70799 - 14.8867 GPa

@Strain 0.0500 - 4.13 %
247.727 - 2159.17 ksi

@Strain 0.0500 - 4.13 %
Average value: 10.1 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Secant Modulus 1.70799 - 14.8867 GPa

@Temperature 0.000 - 200 °C
247.727 - 2159.17 ksi

@Temperature 32.0 - 392 °F
Average value: 10.1 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Secant Modulus 1.70799 - 14.8867 GPa

@Strain 0.0500 - 4.13 %
247.727 - 2159.17 ksi

@Strain 0.0500 - 4.13 %
Average value: 10.1 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..