Mechanical Properties Metric English Comments
Secant Modulus 0.957 GPa

@Strain 1.40 %,
Temperature 100 °C
139 ksi

@Strain 1.40 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Secant Modulus 0.957 GPa

@Strain 1.40 %,
Temperature 100 °C
139 ksi

@Strain 1.40 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
Secant Modulus 0.960 GPa

@Strain 2.00 %,
Temperature 40.0 °C
139 ksi

@Strain 2.00 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..