Polymer Property : Secant Modulus = 13.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 13.7 GPa

@Strain 0.150 %,
Temperature 23.0 °C
1980 ksi

@Strain 0.150 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Secant Modulus 13.7 GPa

@Strain 1.40 %,
Temperature -40.0 °C
1980 ksi

@Strain 1.40 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Secant Modulus 13.7 GPa

@Strain 0.130 %,
Temperature -40.0 °C
1980 ksi

@Strain 0.130 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Secant Modulus 13.7 GPa

@Strain 0.610 %,
Temperature 40.0 °C
1980 ksi

@Strain 0.610 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..