Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 12.5 GPa @Strain 0.225 %, Temperature -40.0 °C |
1810 ksi @Strain 0.225 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |