Polymer Property : Secant Modulus = 11.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 11.6 GPa

@Strain 0.130 %,
Temperature 23.0 °C
1690 ksi

@Strain 0.130 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Secant Modulus 11.6 GPa

@Strain 1.02 %,
Temperature 40.0 °C
1690 ksi

@Strain 1.02 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Secant Modulus 11.6 GPa

@Strain 0.480 %,
Temperature 40.0 °C
1690 ksi

@Strain 0.480 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers