Mechanical Properties Metric English Comments
Secant Modulus 0.076397 GPa

@Strain 35.97 %,
Temperature -40.0 °C
11.081 ksi

@Strain 35.97 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..