Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 11.08 GPa @Strain 0.900 %, Temperature -40.0 °C |
1607 ksi @Strain 0.900 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |