Polymer Property : Secant Modulus = 1.775 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.775 GPa

@Strain 2.00 %,
Temperature 40.0 °C
257.4 ksi

@Strain 2.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Secant Modulus 1.775 GPa

@Strain 2.00 %,
Temperature 40.0 °C
257.4 ksi

@Strain 2.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..