Mechanical Properties Metric English Comments
Secant Modulus 1.75 GPa

@Strain 2.40 %,
Temperature 23.0 °C
254 ksi

@Strain 2.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Secant Modulus 1.75 GPa

@Strain 2.40 %,
Temperature 23.0 °C
254 ksi

@Strain 2.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..
Secant Modulus 1.75 GPa

@Strain 2.63 %,
Temperature 200 °C
254 ksi

@Strain 2.63 %,
Temperature 392 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Secant Modulus 1.75 GPa

@Strain 2.63 %,
Temperature 200 °C
254 ksi

@Strain 2.63 %,
Temperature 392 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Secant Modulus 1.75 GPa

@Strain 4.24 %,
Temperature 0.000 °C
254 ksi

@Strain 4.24 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers