Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.20 GPa @Strain 7.00 %, Temperature 100 °C |
174 ksi @Strain 7.00 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Secant Modulus | 1.20 GPa @Strain 3.50 %, Temperature 80.0 °C |
174 ksi @Strain 3.50 %, Temperature 176 °F |
ISO 11403-1 -2 |