Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.82593 GPa @Strain 4.0748 %, Temperature 80.0 °C |
119.79 ksi @Strain 4.0748 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |