Polymer Property : Secant Modulus = 0.750 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.750 GPa

@Strain 4.20 %,
Temperature 80.0 °C
109 ksi

@Strain 4.20 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Secant Modulus 0.750 GPa

@Strain 5.40 %,
Temperature 40.0 °C
109 ksi

@Strain 5.40 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Secant Modulus 0.750 GPa

@Strain 4.20 %,
Temperature 80.0 °C
109 ksi

@Strain 4.20 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..