Mechanical Properties Metric English Comments
Secant Modulus 0.599 GPa

@Strain 14.97 %,
Temperature -20.0 °C
86.8 ksi

@Strain 14.97 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..