Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.478 GPa @Strain 8.21 %, Temperature 0.000 °C |
69.4 ksi @Strain 8.21 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |