Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 0.401 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.401 GPa

@Strain 15.19 %,
Temperature 23.0 °C
58.2 ksi

@Strain 15.19 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6  (Unverified Data**)
40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..