Mechanical Properties Metric English Comments
Secant Modulus 0.326 GPa

@Strain 4.58579 %,
Temperature 100 °C
47.3 ksi

@Strain 4.58579 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers