Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.293 GPa @Strain 15.2 %, Temperature 40.0 °C |
42.5 ksi @Strain 15.2 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |