Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 6.30 GPa | 914 ksi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |