Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 80.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet)
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet)
Compressive Modulus 0.552 GPa

@Temperature 22.8 °C
80.0 ksi

@Temperature 73.0 °F
ASTM D695
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f..
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE
Compressive Modulus 0.552 GPa
80.0 ksi
Stabilized, typ, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 1/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Compressive Modulus 0.552 GPa
80.0 ksi
ASTM D695
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet)
Copyright © lookpolymers.com All Rights Reserved