Compressive Modulus 7.70 - 18.0 GPa
1120 - 2610 ksi
Average value: 13.2 GPa Grade Count:7
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..