Compressive Modulus 7.60 GPa
1100 ksi
Sawbones E-Glass-Filled Epoxy Sheets
Primary UseE-glass-filled epoxy sheets are primarily used as an alternative test medium to human cortical bone.DescriptionE-glass-filled epoxy sheets are a mixture of short e-glass fibers and epoxy ..
Compressive Modulus 7.60 GPa
1100 ksi
Sawbones Third-Generation Simulated Cortical Bone
E-glass-filled EpoxySawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area h..
Compressive Modulus 7.60 GPa
1100 ksi
Sawbones E-Glass-Filled Epoxy Cylinders
Primary UseE-glass-filled epoxy cylinders are primarily used as an alternative test medium to human cortical bone.DescriptionThey are a mixture of short e-glass fibers and epoxy resin that has been ..
Compressive Modulus 7.60 - 16.7 GPa
1100 - 2420 ksi
Average value: 10.7 GPa Grade Count:5
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..