Mechanical Properties Metric English Comments
Compressive Modulus 0.0460 GPa
6.67 ksi
ASTM D1621
SABIC Innovative Plastics ULTEM Foam XP060 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Compressive Modulus 0.0460 GPa
6.67 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Compressive Modulus 0.0460 - 6.47 GPa
6.67 - 938 ksi
Average value: 3.28 GPa Grade Count:21
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..