Polymer Property : Compressive Modulus = 545 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 3.76 GPa
545 ksi
ASTM D695
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products
Compressive Modulus 3.76 GPa
545 ksi
ASTM D695
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)