Polymer Property : Compressive Modulus = 5.90 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 5.90 GPa
856 ksi
ASTM D695
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. ..