Mechanical Properties Metric English Comments
Compressive Modulus 3.20 GPa
464 ksi
Sample Type A, 1 mm/min; ISO 604:2002
Global EPP PA 66E Extruded Polyamide 66
Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu..