Compressive Modulus 0.300 GPa
43.5 ksi
MarkeTech Resorcinol Formaldehyde Aerogel
Monolithic resorcinol formaldehyde (RF) nanofoams are primarily used as the precursor for carbon nanofoams or when an organic, electrically insulating material is desired. The standard RF nanofoam i..
Compressive Modulus 0.300 GPa
43.5 ksi
Loading, In the Through Plane Direction
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..