Mechanical Properties Metric English Comments
Compressive Modulus 2.942 GPa
426.7 ksi
ASTM D695
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded ..