Mechanical Properties Metric English Comments
Compressive Modulus 2.82 GPa
409 ksi
ASTM D695
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide
Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di..