Mechanical Properties Metric English Comments
Compressive Modulus 2.54 GPa
368 ksi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex