Polymer Property : Compressive Modulus = 343.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 2.365 GPa
343.0 ksi
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam
Eccolite Ultra syntactic foam plug assist materials a new engineered thermoplastic compound incorporating Eccospheres, glass microspheres. It is one of the toughest materials designed for the therm..