Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0250 GPa | 3.63 ksi | perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam AIREX® C51 is a closed-cell polymer foam with outstanding damage tolerance and formability. Its excellent price / performance ratio uniquely qualifies this core material for high-volume sandwich .. |