Mechanical Properties Metric English Comments
Compressive Modulus 3.50 GPa
508 ksi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
Compressive Modulus 3.50 GPa
508 ksi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..