Compressive Modulus 3.3864 GPa

@Temperature 23.0 °C
491.16 ksi

@Temperature 73.4 °F
ASTM D695
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts
Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L