Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 3.34 GPa | 485 ksi | |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |
|||
Compressive Modulus | 3.34 GPa | 485 ksi | TM R050-38 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |