Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.027 GPa @Temperature 23.0 °C |
294.0 ksi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |