Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.97 GPa | 285 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 5/32-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 1.97 GPa | 285 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.97 GPa | 285 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.97 GPa | 285 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/16-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |