Polymer Property : Compressive Modulus = 254 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.75 GPa
254 ksi
Henkel Hysol EA 9330 Paste Adhesive System
Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding