Polymer Property : Compressive Modulus = 2300 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 15.9 GPa

@Temperature 23.9 °C
2300 ksi

@Temperature 75.0 °F
Dry
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..