Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.54 GPa | 224 ksi | ASTM D695 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |