Mechanical Properties Metric English Comments
Compressive Modulus >= 0.150 GPa
>= 21.8 ksi
perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..