Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.7213 GPa @Temperature 23.0 °C |
394.69 ksi @Temperature 73.4 °F |
ASTM D695 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical propertyInformation provided by Daelim H&L |