Polymer Property : Compressive Modulus = 2.48 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 2.48 GPa
360 ksi
ASTM D695
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
Compressive Modulus 2.48 GPa
360 ksi
ASTM D695
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet)
Compressive Modulus 2.48 GPa
359 ksi
ASTM D695
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet)
Compressive Modulus 2.48 GPa
360 ksi
ASTM D695
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Modulus 2.48 GPa
360 ksi
ASTM D695
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Modulus 2.48 GPa
359 ksi
ASTM D695
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per..