Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.413 GPa | 350.0 ksi | ASTM D695 |
Manifattura Cattaneo VESPEL® SP1 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |