Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.067 GPa @Temperature 23.0 °C |
299.8 ksi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |