Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 13.5 GPa @Temperature 75.0 °C |
1960 ksi @Temperature 167 °F |
90º, Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |